| 1. | It can be melted if the PS board stays in
high temperature too long. 75 |
|||||
| 2. | It may be corroded if the blister board and the volatile materials are in direct contact. | |||||
| 3. | The construction of the cell will be ruined when it is laid in the sun for a long time. Besides, the surface will turn out to be yellow. If it is necessary to put the board in the sun for days. it had better be covered with white polythylene film or any light-colored thin materials. The yellow part on the surface should be erased before it glues anything on. | |||||
|
||||||
![]() |
||||||
|
||||||
| WIN-LUCK board contains fire-resistant substance. so it prevents from catching on fire through a tongue of flame; nevertheless, its materials are combustible. No matter where you lay the WIN-LUCK, it should not be exposed to the flame. | ||||||